8 Year Exporter P91 Alloy Pipe - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe

Short Description:


Product Detail

Product Tags

Related Video

Feedback (2)

We not only will try our greatest to offer you excellent services to just about every client, but also are ready to receive any suggestion offered by our buyers for Alloy Steel Pipe A210 , 12crmov Alloy Tube , Alloy Steel Pipe A335 P91 , Sincerely hope to build long term business relationships with you and we will do our best service for you.
8 Year Exporter P91 Alloy Pipe - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe Detail:

Overview

Application

It is mainly used to make high-quality seamless carbon steel, for boiler pipes, super heat pipes

for bolier industry , heat changer pipe etc. With difference sizes and thickness

Main Grade

Grade of high-quality carbon boiler steel: GrA, GrC

Chemical Component

Element Grade A Grade C
C ≤0.27 ≤0.35
Mn ≤0.93 0.29-1.06
P ≤0.035 ≤0.035
S ≤0.035 ≤0.035
Si ≥ 0.1 ≥ 0.1

A For each reduction of 0.01 % below the specified carbon maximum, an increase of 0.06 % manganese above the specified maximum will be permitted up to a maximum of 1.35 %.

Mechanical Property

Grade A Grade C
Tensile Strength ≥ 415 ≥ 485
Yield Strength ≥ 255 ≥ 275
  Elongation rate ≥ 30 ≥ 30

Test Requirement

Hydraustatic Test:

The Steel Pipe Should Be Tested Hydraulically One By One. The Maximum Test Pressure Is 20 MPa. Under The Test Pressure, The Stabilization Time Should Be Not Less Than 10 S, And The Steel Pipe Should Not Leak.

After The User Agrees, The Hydraulic Test Can Be Replaced By Eddy Current Testing Or Magnetic Flux Leakage Testing.

Flattening Test:

Tubes With An Outer Diameter Greater Than 22 Mm Shall Be Subjected To A Flattening Test. No Visible Delamination, White Spots, Or Impurities Should Occur During The Entire Experiment.

Flaring Test:

According To The Requirements Of The Purchaser And Stated In The Contract, The Steel Pipe With Outer Diameter ≤76mm And Wall Thickness ≤8mm Can Be Done Flaring Test . The Experiment Was Performed At Room Temperature With A Taper Of 60 °. After The Flaring, The Flaring Rate Of The Outer Diameter Should Meet The Requirements Of The Following Table, And The Test Material Must Not Show Cracks Or Rips

Hardness Test:

Brinell or Rockwell hardness tests shall be made on specimens from two tubes from each lot

Product Detail

Boiler Tube


1


GB/T5310-2017

A106 Boiler Pipe


ASME SA-106/SA-106M-2015


carbon steel pipe


ASTMA210(A210M)-2012


eamless steel tubes for normal structure


ASME SA-213/SA-213M


boiler pipe IBR


ASTM A335/A335M-2018


Product detail pictures:

8 Year Exporter P91 Alloy Pipe -
 Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe detail pictures

8 Year Exporter P91 Alloy Pipe -
 Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe detail pictures

8 Year Exporter P91 Alloy Pipe -
 Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe detail pictures


Related Product Guide:

We know that we only thrive if we can guarantee our combined price competiveness and quality advantageous at the same time for 8 Year Exporter P91 Alloy Pipe - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe , The product will supply to all over the world, such as: Finland , Toronto , British , Furthermore, all of our products are manufactured with advanced equipment and strict QC procedures in order to ensure high quality. If you are interested in any of our products, please don't hesitate to contact us. We will do our best to meet your needs.
  • We are really happy to find such a manufacturer that ensuring product quality at the same time the price is very cheap.
    5 Stars By Philipppa from Yemen - 2018.06.03 10:17
    High production efficiency and good product quality, fast delivery and completed after-sale protection, a right choice, a best choice.
    5 Stars By Jean Ascher from Bangkok - 2018.11.28 16:25
    Write your message here and send it to us