Factory Price China ASME SA335 P5 P9 P11 P12 P22 P91 P92 Alloy Seamless Steel Tube Smls Pipe

Short Description:

ASTM A335 standard high Temperature boiler pipe seamless alloy pipe with IBR certifiaction

Seamless alloy pipe for boiler ,heat exchanger etc industry

 


  • Payment: 30% deposit, 70% L/C or B/L copy or 100% L/C at sight
  • Min.Order Quantity: 1 PC
  • Supply Ability: Annual 20000 Tons Inventory of Steel Pipe
  • Lead Time: 7-14 days if in stock, 30-45 days to produce
  • Packing: Black Vanishing, bevel and cap for every single pipe; OD below 219mm need to pack in bundle, and each bundle no exceed 2 tons.
  • Product Detail

    Product Tags

    Application

    It is mainly used to make high-quality alloy steel boiler pipe , heat exchanged pipe, high pressure steam pipe for petroleum and chemical industry

    Main Grade

    Grade of high-quality alloy pipe :P1,P2,P5,P9,P11,P22,P91,P92 etc

    Main Market

    India, UAE , Pakistian

    For  Inida market main Grade steel is P11, P22, p9, P5, P91.

    ASTM A335 P9  is equal to GB9948 or GB 6479 1Cr9Mo

    ASTM A335 P22 is equal to GB5310 12Cr2MoG

    ASTM A335 P11 is equal to GB5310 14Cr1MoG

    ASTM A335 P5 is equal to  GB5310 1Cr5MoG

    ASTM A335 P91 is equal to GB5310 10Cr9Mo1VNbN

    Differece of GB9948 and GB6479 in Application:

    GB9948 is Seamless Steel Tubes For Petroleum Cracking

    GB6479 is Seamless steel tubes for high-pressure For chemical fertilizer equipments

    Sequence No.  Items to test Test method Quantity for sampling Standard
    1 Chemical composition GB/T222
    GB/T223
    GB/4336
    One sample for each furnace GB6479/GB9948
    2 Tensile test  GB/T 228 One sample respectively taken from
    two tubes of each batch
    GB6479/GB9948
    3 Impact test GB/T 229 Three samples respectively taken
    from two tubes of each batch
    GB6479/GB9948
    4 Hydraulic test GB/T 241 Piece by piece GB6479/GB9948
    5 Press-flat test GB/T 246 One sample respectively taken from
    two tubes of each batch
    GB6479/GB9948
    6 Opening expansion test GB/T 242 GB6479/GB9948
    7 Low-fold test GB/T 226
    GB/T 1979
    GB6479/GB9948
    8 Non-metal inclusion GB/T 10561 GB6479/GB9948
    9 Ultrasonic testing GB/T 5777 Piece by piece GB6479/GB9948
    10 Eddy testing GB/T 7735 GB6479/GB9948
    11 Leaking magnetic testing GB/T 12606 GB6479/GB9948
    12 Hardness Test GB/T231.1 One sample respectively taken from
    two tubes of each batch
    GB9949

    Chemical Component

    GB6479 C Si Mn Cr Mo V Ti NB Ni Cu P S
    1Cr5Mo ≤0.15 ≤0.5 ≤0.6 4-6 0.45-0.6 / / / ≤0.6 ≤0.2 ≤0.03 ≤0.03
    GB9948 C Si Mn Cr Mo V Ti NB Ni Cu P S
    1Cr5Mo ≤0.15 ≤0.5 ≤0.6 4-6 0.45-0.6 / / / ≤0.6 ≤0.2 ≤0.03 ≤0.02

    Chemical Component

    Grade UN C≤ Mn P≤ S≤ Si≤ Cr Mo
    Sequiv.
    P1 K11522 0.10~0.20 0.30~0.80 0.025 0.025 0.10~0.50 0.44~0.65
    P2 K11547 0.10~0.20 0.30~0.61 0.025 0.025 0.10~0.30 0.50~0.81 0.44~0.65
    P5 K41545 0.15 0.30~0.60 0.025 0.025 0.5 4.00~6.00 0.44~0.65
    P5b K51545 0.15 0.30~0.60 0.025 0.025 1.00~2.00 4.00~6.00 0.44~0.65
    P5c K41245 0.12 0.30~0.60 0.025 0.025 0.5 4.00~6.00 0.44~0.65
    P9 S50400 0.15 0.30~0.60 0.025 0.025 0.50~1.00 8.00~10.00 0.44~0.65
    P11 K11597 0.05~0.15 0.30~0.61 0.025 0.025 0.50~1.00 1.00~1.50 0.44~0.65
    P12 K11562 0.05~0.15 0.30~0.60 0.025 0.025 0.5 0.80~1.25 0.44~0.65
    P15 K11578 0.05~0.15 0.30~0.60 0.025 0.025 1.15~1.65 0.44~0.65
    P21 K31545 0.05~0.15 0.30~0.60 0.025 0.025 0.5 2.65~3.35 0.80~1.60
    P22 K21590 0.05~0.15 0.30~0.60 0.025 0.025 0.5 1.90~2.60 0.87~1.13
    P91 K91560 0.08~0.12 0.30~0.60 0.02 0.01 0.20~0.50 8.00~9.50 0.85~1.05
    P92 K92460 0.07~0.13 0.30~0.60 0.02 0.01 0.5 8.50~9.50 0.30~0.60

    A New designation established in accordance with Practice E 527 and SAE J1086, Practice for Numbering Metals and Alloys (UNS). B Grade P 5c shall have a titanium content of not less than 4 times the carbon content and not more than 0.70 %; or a columbium content of 8 to 10 times the carbon content.

    Mechanical Property

    Mechanical properties  P1,P2  P12  P23  P91  P92,P11  P122
     Tensile strength  380  415  510  585  620  620
     Yield strength  205  220  400  415  440  400

    Heat Treatment

    Grade Heat Treatment Type Normalizing Temperature Range F [C] Subcritical Annealing or Tempering
    P5, P9, P11, and P22 Temperature Range F [C]
    A335 P5 (b,c) Full or Isothermal Anneal
    Normalize and Temper ***** 1250 [675]
    Subcritical Anneal (P5c only) ***** 1325 – 1375 [715 - 745]
    A335 P9 Full or Isothermal Anneal
    Normalize and Temper ***** 1250 [675]
    A335 P11 Full or Isothermal Anneal
    Normalize and Temper ***** 1200 [650]
    A335 P22 Full or Isothermal Anneal
    Normalize and Temper ***** 1250 [675]
    A335 P91 Normalize and Temper 1900-1975 [1040 - 1080] 1350-1470 [730 - 800]
    Quench and Temper 1900-1975 [1040 - 1080] 1350-1470 [730 - 800]

    Test Requirement

    In addition to ensuring chemical composition and mechanical properties, hydrostatic tests are performed one by one,  Nondestructive Examination ,Product Analysis , Metal Structure and Etching Tests ,Flattening test etc.

    Supply Ability

    Supply Ability: 2000 Tons Per Month Per Grade of ASTM A335  Alloy Steel Pipe

    Packaging

    In Bundles And In Strong Wooden Box

    Delivery

    7-14 days if in stock, 30-45 days to produce

    Payment

    30% depsoit, 70% L/C or B/L copy   or  100% L/C at sight

    Product Detail

    Boiler Tube


    GB/T5310-2017


    ASME SA-106/SA-106M-2015

    carbon steel pipe


    ASTMA210(A210M)-2012


    ASME SA-213/SA-213M


    ASTM A335/A335M-2018