Factory Selling China ASTM A335 P12 P22 P11 Cold Rolled or Cold Drawn Seamless Alloy Steel Boiler Pipe
Overview
We stick to our company spirit of "Quality, Effectiveness, Innovation and Integrity". We purpose to create far more value for our customers with our abundant resources, sophisticated machinery, experienced workers and exceptional expert services for carbon steel and Cr Mo alloy steel boiler pipe. To improved expand market. Whether selecting a current product from our catalog or seeking engineering assistance for your application, you can talk to our customer service center about your sourcing requirements. We've been looking forward to cooperating with friends from all over the world.
Application
It is mainly used to make high-quality alloy steel boiler pipe , heat exchanged pipe, high pressure steam pipe for petroleum and chemical industry
Main Grade
Grade of high-quality alloy pipe :P1,P2,P5,P9,P11,P22,P91,P92 etc
Chemical Component
Grade | UN | C≤ | Mn | P≤ | S≤ | Si≤ | Cr | Mo |
Sequiv. | ||||||||
P1 | K11522 | 0.10~0.20 | 0.30~0.80 | 0.025 | 0.025 | 0.10~0.50 | – | 0.44~0.65 |
P2 | K11547 | 0.10~0.20 | 0.30~0.61 | 0.025 | 0.025 | 0.10~0.30 | 0.50~0.81 | 0.44~0.65 |
P5 | K41545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P5b | K51545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.00~2.00 | 4.00~6.00 | 0.44~0.65 |
P5c | K41245 | 0.12 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P9 | S50400 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.50~1.00 | 8.00~10.00 | 0.44~0.65 |
P11 | K11597 | 0.05~0.15 | 0.30~0.61 | 0.025 | 0.025 | 0.50~1.00 | 1.00~1.50 | 0.44~0.65 |
P12 | K11562 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 0.80~1.25 | 0.44~0.65 |
P15 | K11578 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.15~1.65 | – | 0.44~0.65 |
P21 | K31545 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 2.65~3.35 | 0.80~1.60 |
P22 | K21590 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 1.90~2.60 | 0.87~1.13 |
P91 | K91560 | 0.08~0.12 | 0.30~0.60 | 0.02 | 0.01 | 0.20~0.50 | 8.00~9.50 | 0.85~1.05 |
P92 | K92460 | 0.07~0.13 | 0.30~0.60 | 0.02 | 0.01 | 0.5 | 8.50~9.50 | 0.30~0.60 |
A New designation established in accordance with Practice E 527 and SAE J1086, Practice for Numbering Metals and Alloys (UNS). B Grade P 5c shall have a titanium content of not less than 4 times the carbon content and not more than 0.70 %; or a columbium content of 8 to 10 times the carbon content.
Mechanical Property
Mechanical properties | P1,P2 | P12 | P23 | P91 | P92,P11 | P122 |
Tensile strength | 380 | 415 | 510 | 585 | 620 | 620 |
Yield strength | 205 | 220 | 400 | 415 | 440 | 400 |
Heat Treatment
Grade | Heat Treatment Type | Normalizing Temperature Range F [C] | Subcritical Annealing or Tempering |
P5, P9, P11, and P22 | Temperature Range F [C] | ||
A335 P5 (b,c) | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
Subcritical Anneal (P5c only) | ***** | 1325 – 1375 [715 - 745] | |
A335 P9 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
A335 P11 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1200 [650] | |
A335 P22 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
A335 P91 | Normalize and Temper | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
Quench and Temper | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
Test Requirement
In addition to ensuring chemical composition and mechanical properties, hydrostatic tests are performed one by one, Nondestructive Examination ,Product Analysis , Metal Structure and Etching Tests ,Flattening test etc.
Supply Ability
Supply Ability: 2000 Tons Per Month Per Grade of ASTM A335 Alloy Steel Pipe
Packaging
In Bundles And In Strong Wooden Box
Delivery
7-14 days if in stock, 30-45 days to produce
Payment
30% depsoit, 70% L/C or B/L copy or 100% L/C at sight