Hot Dipped Galvanized Steel Pipe - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe

Short Description:


Product Detail

Product Tags

Related Video

Feedback (2)

Every member from our high efficiency sales team values customers' needs and business communication for Low Temperature Steel Pipe , Electric Furnace Steelmaking , structural seamless steel tubes , We are willing to give you the lowest price in the market, best quality and very nice sales service.Welcome to do bussines with us,let's be double win.
Hot Dipped Galvanized Steel Pipe - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe Detail:

Overview

Application

It is mainly used to make high-quality seamless carbon steel, for boiler pipes, super heat pipes

for bolier industry , heat changer pipe etc. With difference sizes and thickness

Main Grade

Grade of high-quality carbon boiler steel: GrA, GrC

Chemical Component

Element Grade A Grade C
C ≤0.27 ≤0.35
Mn ≤0.93 0.29-1.06
P ≤0.035 ≤0.035
S ≤0.035 ≤0.035
Si ≥ 0.1 ≥ 0.1

A For each reduction of 0.01 % below the specified carbon maximum, an increase of 0.06 % manganese above the specified maximum will be permitted up to a maximum of 1.35 %.

Mechanical Property

Grade A Grade C
Tensile Strength ≥ 415 ≥ 485
Yield Strength ≥ 255 ≥ 275
  Elongation rate ≥ 30 ≥ 30

Test Requirement

Hydraustatic Test:

The Steel Pipe Should Be Tested Hydraulically One By One. The Maximum Test Pressure Is 20 MPa. Under The Test Pressure, The Stabilization Time Should Be Not Less Than 10 S, And The Steel Pipe Should Not Leak.

After The User Agrees, The Hydraulic Test Can Be Replaced By Eddy Current Testing Or Magnetic Flux Leakage Testing.

Flattening Test:

Tubes With An Outer Diameter Greater Than 22 Mm Shall Be Subjected To A Flattening Test. No Visible Delamination, White Spots, Or Impurities Should Occur During The Entire Experiment.

Flaring Test:

According To The Requirements Of The Purchaser And Stated In The Contract, The Steel Pipe With Outer Diameter ≤76mm And Wall Thickness ≤8mm Can Be Done Flaring Test . The Experiment Was Performed At Room Temperature With A Taper Of 60 °. After The Flaring, The Flaring Rate Of The Outer Diameter Should Meet The Requirements Of The Following Table, And The Test Material Must Not Show Cracks Or Rips

Hardness Test:

Brinell or Rockwell hardness tests shall be made on specimens from two tubes from each lot

Product Detail

Boiler Tube


1


GB/T5310-2017

A106 Boiler Pipe


ASME SA-106/SA-106M-2015


carbon steel pipe


ASTMA210(A210M)-2012


eamless steel tubes for normal structure


ASME SA-213/SA-213M


boiler pipe IBR


ASTM A335/A335M-2018


Product detail pictures:

Hot Dipped Galvanized Steel Pipe -
 Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe detail pictures

Hot Dipped Galvanized Steel Pipe -
 Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe detail pictures

Hot Dipped Galvanized Steel Pipe -
 Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe detail pictures


Related Product Guide:

Being supported by an advanced and specialist IT team, we could give technical support on pre-sales & after-sales services for Hot Dipped Galvanized Steel Pipe - Seamless Medium carbon steel boiler and Superheat tubes ASTM A210 standard – Sanonpipe , The product will supply to all over the world, such as: Bolivia , Mombasa , luzern , You can let us know your idea to develop unique design for your own model to prevent too much similar parts in the market! We will offer our best service to satisfy all your needs! Please contact us right away!
  • The customer service staff's attitude is very sincere and the reply is timely and very detailed, this is very helpful for our deal,thank you.
    5 Stars By Frank from Argentina - 2018.11.06 10:04
    We have worked with many companies, but this time is the best,detailed explanation, timely delivery and quality qualified, nice!
    5 Stars By Caroline from New Orleans - 2018.09.12 17:18
    Write your message here and send it to us