Main Grade
Grade :J55,K55,N80,L80,P110, etc
Chemical Component
|
Mechanical Property
Grade |
Type |
Total Elongation Under Load |
Yield Strength |
Tensile Strength |
Hardness a,c |
Specified Wall Thickness |
Allowable Hardness Variation b |
||
|
|
|
|
|
|
|
|
||
|
|
|
min |
max |
|
HRC |
HBW |
mm |
HRC |
H40 |
— |
0.5 |
276 |
552 |
414 |
— |
— |
— |
— |
J55 |
— |
0.5 |
379 |
552 |
517 |
— |
— |
— |
— |
K55 |
— |
0.5 |
379 |
552 |
655 |
— |
— |
— |
— |
N80 |
1 |
0.5 |
552 |
758 |
689 |
— |
— |
— |
— |
N80 |
Q |
0.5 |
552 |
758 |
689 |
— |
— |
— |
— |
R95 |
— |
0.5 |
655 |
758 |
724 |
— |
— |
— |
— |
L80 |
1 |
0.5 |
552 |
655 |
655 |
23.0 |
241.0 |
— |
— |
L80 |
9Cr |
0.5 |
552 |
655 |
655 |
23.0 |
241.0 |
— |
— |
L80 |
l3Cr |
0.5 |
552 |
655 |
655 |
23.0 |
241.0 |
— |
— |
C90 |
1 |
0.5 |
621 |
724 |
689 |
25.4 |
255.0 |
≤12.70 |
3.0 |
12.71 to 19.04 |
4.0 |
||||||||
19.05 to 25.39 |
5.0 |
||||||||
≥25.4 |
6.0 |
||||||||
T95 |
1 |
0.5 |
655 |
758 |
724 |
25.4 |
255 |
≤12.70 |
3.0 |
12.71 to 19.04 |
4.0 |
||||||||
19.05 to 25.39 |
5.0 |
||||||||
≥25.4 |
6.0 |
||||||||
C110 |
— |
0.7 |
758 |
828 |
793 |
30.0 |
286.0 |
≤12.70 |
3.0 |
12.71 to 19.04 |
4.0 |
||||||||
19.05 to 25.39 |
5.0 |
||||||||
≥25.4 |
6.0 |
||||||||
P110 |
— |
0.6 |
758 |
965 |
862 |
— |
— |
— |
— |
Q125 |
1 |
0.65 |
862 |
1034 |
931 |
b |
— |
≤12.70 |
3.0 |
12.71 to 19.04 |
4.0 |
||||||||
19.05 |
5.0 |
||||||||
a In case of dispute, laboratory Rockwell C hardness testing shall be used as the referee method. | |||||||||
b No hardness limits are specified, but the maximum variation is restricted as a manufacturing control in accordance with 7.8 and 7.9. | |||||||||
c For through-wall hardness tests of Grades L80 (all types), C90, T95 and C110, the requirements stated in HRC scale are for maximum mean hardness number. |
Test Requirement
In addition to ensuring chemical composition and mechanical properties, hydrostatic tests are performed one by one, and flaring and flattening tests are performed. . In addition, there are certain requirements for the microstructure, grain size, and decarburization layer of the finished steel pipe.
Supply Ability
Supply Ability: 500 Tons Per Month Per Grade of API 5CT PIPE
Packaging
In Bundles And In Strong Wooden Box
Delivery
7-14 days if in stock, 30-45 days to produce
Payment
30% depsoit, 70% L/C or B/L copy or 100% L/C at sight
Product Detail
Petroleum Pipes Structure Pipes
API 5L
API 5CT
Product detail pictures:
Related Product Guide:
We not only will try our greatest to supply outstanding services to every shopper, but also are ready to receive any suggestion offered by our buyers for OEM Manufacturer Alloy Steel Pipe A333 - Specification for Casing and Tubing API SPECIFICATION 5CT NINTH EDITION-2012 – Sanonpipe , The product will supply to all over the world, such as: venezuela , Austria , Greece , We put the product quality and customer's benefits to the first place. Our experienced salesmen supply prompt and efficient service. Quality control group make sure the best quality. We believe quality comes from detail. If you have demand, allow us to work together to get success.
By Lulu from Mexico - 2017.01.11 17:15
Product variety is complete, good quality and inexpensive, the delivery is fast and transport is security, very good, we are happy to cooperate with a reputable company!
By Nana from Brasilia - 2017.12.02 14:11