With this motto in mind, we now have turn out to be amongst quite possibly the most technologically innovative, cost-efficient, and price-competitive manufacturers for High Pressure Alloy Steel Seamless Boiler Pipe, Be sure to experience free to make contact with us at any time. We're going to reply you when we receive your inquiries. Please note that samples are available before we start our business. We are going to not only continuously introduce technical guidance of experts from both home and abroad, but also develop the new and advanced products constantly to satisfactorily meet the needs of our clients all over the world.
Application
It is mainly used to make high-quality alloy steel boiler pipe , heat exchanged pipe, high pressure steam pipe for petroleum and chemical industry
Main Grade
Grade of high-quality alloy pipe :P1,P2,P5,P9,P11,P22,P91,P92 etc
Chemical Component
Grade | UN | C≤ | Mn | P≤ | S≤ | Si≤ | Cr | Mo |
Sequiv. | ||||||||
P1 | K11522 | 0.10~0.20 | 0.30~0.80 | 0.025 | 0.025 | 0.10~0.50 | – | 0.44~0.65 |
P2 | K11547 | 0.10~0.20 | 0.30~0.61 | 0.025 | 0.025 | 0.10~0.30 | 0.50~0.81 | 0.44~0.65 |
P5 | K41545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P5b | K51545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.00~2.00 | 4.00~6.00 | 0.44~0.65 |
P5c | K41245 | 0.12 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P9 | S50400 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.50~1.00 | 8.00~10.00 | 0.44~0.65 |
P11 | K11597 | 0.05~0.15 | 0.30~0.61 | 0.025 | 0.025 | 0.50~1.00 | 1.00~1.50 | 0.44~0.65 |
P12 | K11562 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 0.80~1.25 | 0.44~0.65 |
P15 | K11578 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.15~1.65 | – | 0.44~0.65 |
P21 | K31545 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 2.65~3.35 | 0.80~1.60 |
P22 | K21590 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 1.90~2.60 | 0.87~1.13 |
P91 | K91560 | 0.08~0.12 | 0.30~0.60 | 0.02 | 0.01 | 0.20~0.50 | 8.00~9.50 | 0.85~1.05 |
P92 | K92460 | 0.07~0.13 | 0.30~0.60 | 0.02 | 0.01 | 0.5 | 8.50~9.50 | 0.30~0.60 |
A New designation established in accordance with Practice E 527 and SAE J1086, Practice for Numbering Metals and Alloys (UNS). B Grade P 5c shall have a titanium content of not less than 4 times the carbon content and not more than 0.70 %; or a columbium content of 8 to 10 times the carbon content.
Mechanical Property
Mechanical properties | P1,P2 | P12 | P23 | P91 | P92,P11 | P122 |
Tensile strength | 380 | 415 | 510 | 585 | 620 | 620 |
Yield strength | 205 | 220 | 400 | 415 | 440 | 400 |
Heat Treatment
Grade | Heat Treatment Type | Normalizing Temperature Range F [C] | Subcritical Annealing or Tempering |
P5, P9, P11, and P22 | Temperature Range F [C] | ||
A335 P5 (b,c) | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
Subcritical Anneal (P5c only) | ***** | 1325 – 1375 [715 - 745] | |
A335 P9 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
A335 P11 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1200 [650] | |
A335 P22 | Full or Isothermal Anneal | ||
Normalize and Temper | ***** | 1250 [675] | |
A335 P91 | Normalize and Temper | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
Quench and Temper | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
Test Requirement
In addition to ensuring chemical composition and mechanical properties, hydrostatic tests are performed one by one, Nondestructive Examination ,Product Analysis , Metal Structure and Etching Tests ,Flattening test etc.
Supply Ability
Supply Ability: 2000 Tons Per Month Per Grade of ASTM A335 Alloy Steel Pipe
Packaging
In Bundles And In Strong Wooden Box
Delivery
7-14 days if in stock, 30-45 days to produce
Payment
30% depsoit, 70% L/C or B/L copy or 100% L/C at sight