Wholesale OEM/ODM China 12cr1MOV Seamless Boiler Pipe
Bear “Customer first, Excellent first” in mind, we work closely with our shoppers and supply them with efficient and specialist services for Wholesale OEM/ODM China 12cr1MOV Seamless Boiler Pipe, Our main objectives are to offer our prospects around the globe with good quality, competitive price, happy delivery and superb products and services.
Bear “Customer first, Excellent first” in mind, we work closely with our shoppers and supply them with efficient and specialist services for 12cr1MOV Alloy Seamless Steel Tube, China 12cr1MOV Seamless Boiler Pipe, Due to the changing trends in this field, we involve ourselves into products trade with dedicated efforts and managerial excellence. We maintain timely delivery schedules, innovative designs, quality and transparency for our customers. Our moto is to deliver quality products within stipulated time.
Overview
Standard: GB9948-2006 | Heat Treatment: Annealing/normalizing/Tempering |
Grade Group: 10、12CrMo、15CrMo, 07Crl9Nil0, etc | Outer Diameter(Round): 10 – 1000 Mm |
Thickness: 1 – 100 mm | Application: heat exchange tubes |
Outer Diameter(Round): 10 – 1000 mm | Surface Treatment: As Customer’s Requirement |
Length: Fixed length or random length | Technique: Hot Rolled |
Section Shape: Round | Special Pipe: Thick Wall Pipe |
Place of Origin: China | Usage: heat exchange tubes |
Certification: ISO9001:2008 | Test:UT/MT |
Application
Seamless steel tubes for petroleum cracking are applicable to seamless steel tubes for furnace tubes, heat exchange tubes and pressure pipes in petrochemical industry.
High quality carbon structural steel grades are 20g, 20mng and 25mng.
Alloy structural steel grades: 15mog, 20mog, 12crmog
15CrMoG、12Cr2MoG、12CrMoVG, etc
Main Grade
Grade of high-quality carbon structural steel: 10#、20#
High quality carbon structural steel grades : 20g, 20mng and 25mng
Alloy structural steel grades: 15mog, 20mog, 12crmog, 15CrMoG、12Cr2MoG,etc
Chemical Component
No | Grade | Chemical Component % | |||||||||||
C | Si | Mn | Cr | Mo | Ni | Nb | Ti | V | Cu | P | S | ||
≤ | |||||||||||||
High Quality Carbon Structural Steel | 10 | 0. 07-0.13 | 0.17 -0. 37 | 0.35 -0.65 | <0.15 | <0.15 | <0. 25 | — | — | <0. 08 | <0. 20 | 0. 025 | 0. 015 |
20 | 0.17-0. 23 | 0.17 -0. 37 | 0.35 -0.65 | <0. 25 | <0.15 | <0. 25 | — | — | <0. 08 | <0. 20 | 0. 025 | 0. 015 | |
Alloy Structural Steel | 12CrMo | 0. 08-0.15 | 0.17 -0.37 | 0. 40-0. 70 | 0. 40-0. 70 | 0. 40 -0.55 | <0. 30 | — | — | 一 | <0. 20 | 0. 025 | 0. 015 |
15CrMo | 0.12 -0.18 | 0.17-0. 37 | 0.40 -0. 70 | 0. 80-1.1 | 0. 40-0.55 | <0. 30 | — | — | 一 | <0. 20 | 0. 025 | 0. 015 | |
12CrlMo | 0. 08 -0.15 | 0.50 -1. 00 | 0. 30-0.6 | 1.00-1. 50 | 0.45 -0.65 | <0. 30 | — | — | — | <0, 20 | 0. 025 | 0. 015 | |
12CrlMoV | 0. 08-0.15 | 0.17-0. 37 | 0. 40-0. 70 | 0.90-1.2 | 0. 25 -0.35 | <0. 30 | — | — | 0.15 -0. 30 | <0. 20 | 0.025 | 0. 010 | |
12Cr2Mo | 0.08-0.15 | <0. 50 | 0. 40-0. 60 | 2. 00-2. 50 | 0. 90-1.13 | <0. 30 | — | — | 一 | <0. 20 | 0. 025 | 0. 015 | |
12Cr5MoI | <0.15 | <0. 50 | 0.30-0.6 | 4. 00-6 | 0. 45 -0. 60 | <0. 60 | — | — | <0. 20 | 0. 025 | 0. 015 | ||
12Cr5MoNT | |||||||||||||
12Cr9MoI | <0.15 | 0. 25-1. 00 | 0. 30-0. 60 | 8.00 -10. 00 | 0. 90-1.1 | <0. 60 | — | — | — | <0. 20 | 0. 025 | 0, 015 | |
12Cr9MoNT | |||||||||||||
Stainless Heat Resistant Steel | 07Crl9Nil0 | 0. 04-0.1 | <1. 00 | <2. 00 | 18. 00-20. 00 | — | 8. 00-11 | — | — | — | — | 0. 030 | 0. 015 |
07Crl8NillNb | 0. 04-0.1 | <1. 00 | <2. 00 | 17. 00-19. 00 | — | 9.00-12. 00 | 8C-1.1 | — | — | — | 0. 030 | 0. 015 | |
07Crl9NillTi | 0. 04-0.1 | <0. 75 | <2. 00 | 17.00-20. 00 | — | 9. 00~13. 00 | — | 4C-0. 60 | 一 | 一 | 0.03 | 0. 015 | |
022Crl7Nil2Mo2 | <0. 030 | <1. 00 | <2. 00 | 16. 00-18. 00 | 2. 00-3. 00 | 10. 00 -14. 00 | — | 一 | 一 | — | 0.03 | 0. 015 |
Mechanical Property
No | Tensile MPa |
Yield MPa |
Elong after fracture A/% | Shork absorption energy kv2/j | Brinell hardness number | ||
portrait | transver | portrait | transver | ||||
not less than | no more than | ||||||
10 | 335〜475 | 205 | 25 | 23 | 40 | 27 | |
20 | 410〜550 | 245 | 24 | 22 | 40 | 27 | |
12CrMo | 410〜560 | 205 | 21 | 19 | 40 | 27 | 156 HBW |
15CrMo | 440〜640 | 295 | 21 | 19 | 40 | 27 | 170 HBW |
12CrlMo | 415〜560 | 205 | 22 | 20 | 40 | 27 | 163 HBW |
12CrlMoV | 470〜640 | 255 | 21 | 19 | 40 | 27 | 179 HBW |
12Cr2Mo | 450~600 | 280 | 22 | 20 | 40 | 27 | 163 HBW |
12Cr5MoI | 415〜590 | 205 | 22 | 20 | 40 | 27 | 163 HBW |
12Cr5MoNT | 480〜640 | 280 | 20 | 18 | 40 | 27 | — |
12Cr9MoI | 460〜640 | 210 | 20 | 18 | 40 | 27 | 179 HBW |
12Cr9MoNT | 590—740 | 390 | 18 | 16 | 40 | 27 | |
O7Crl9NilO | 2520 | 205 | 35 | 187 HBW | |||
07Crl8NillNb | >520 | 205 | 35 | — | 187 HBW | ||
07Crl9NillTi | >520 | 205 | 35 | — | — | 187 HBW | |
022Crl7Nil2Mo2 | >485 | 170 | 35 | 一 | — | 187 HBW | |
For steel with wall thickness less than 5mm tube do not make hardness experiment |
Test Requirement
Hydraulic test
Hydraulic test shall be carried out for steel pipes one by one. The maximum test pressure is 20 MPa. Under the test pressure, the stabilization time shall not be less than 10 s, and leakage of steel pipe is not allowed.
Flattening test
Flattening test shall be conducted for steel pipe with outer diameter greater than 22 mm
Flaring test
High quality carbon structural steel and stainless (heat-resistant) steel pipes with an outer diameter of not more than 76 mm and a wall thickness of not more than 8 mm shall be subject to expanding test. The flaring test shall be carried out at room temperature. The outer diameter flaring rate of the sample after the top core taper is 60% of the flaring shall meet the requirements of table 7. No cracks or cracks are allowed on the sample after the flaring. According to the requirements of the demander and noted in the contract, the alloy structural steel can also be used for expanding test.
Nondestructive teste
The steel pipes shall be subject to ultrasonic flaw detection one by one in accordance with the provisions of GB / T 5777-2008. According to the requirements of the demander, other non-destructive tests can be added after negotiation between the supplier and the demander and indicated in the contract.
Intergranular corrosion test
Intergranular corrosion test shall be conducted for stainless (heat-resistant) steel pipe. The test method shall be in accordance with the provisions of Chinese method E in GB / T 4334-2008, and intergranular corrosion tendency is not allowed after the test.
After negotiation between the supplier and the demander, and noted in the contract, the demander can designate other corrosion test methods.
Product Detail
mechanical/Chemical&Fertilizer Pipes
GB/T8162-2008
ASTM_A519-2006
BS EN 10210-1-2006
ASTM A53A53M-2012
GB9948-2006
GB6479-2013
GB/T 17396-2009
Bear “Customer first, Excellent first” in mind, we work closely with our shoppers and supply them with efficient and specialist services for Wholesale OEM/ODM China 12cr1MOV Seamless Boiler Pipe, Our main objectives are to offer our prospects around the globe with good quality, competitive price, happy delivery and superb products and services.
Wholesale OEM/ODM China 12cr1MOV Seamless Boiler Pipe, 12cr1MOV Alloy Seamless Steel Tube, Due to the changing trends in this field, we involve ourselves into products trade with dedicated efforts and managerial excellence. We maintain timely delivery schedules, innovative designs, quality and transparency for our customers. Our moto is to deliver quality products within stipulated time.
Oil, petrochemical, high pressure boiler, special use of seamless tube boiler seamless tube, geological seamless steel tube and oil seamless tube.
Chemical Component
brand | Chemical Component(%) | ||||||||
C | Mn | Si | Cr | Mo | Ni | Nb+Ta | S | P | |
15CrMo | 0.12~0.18 | 0.40~0.70 | 0.17~0.37 | 0.80~1.10 | 0.40~0.55 | ≤0.30 | _ | ≤0.035 | ≤0.035 |
Mechanical Property
brand | Tensile MPa |
Yield MPa |
Elongation(%) |
15CrMo | 440~640 | 295 | 22 |