Sina ASME SA335 P5 P9 P11 P12 P22 P91 P92 Seamless Steel tube Smls Pipe
Applicationem
Maxime adhibetur ut mixturam ferro boiler fistulam altae qualitatem, fistulam caloris commutatam, altam pressuram vaporis fistulae petrolei et industria chemica
Principalis Gradus
Gradus summus qualitas organi mixturae : P1, P2, P5, P9, P11, P22, P91, P92 etc.
Principalis Market
India, UAE, Pakistian
Nam Inida mercatus principalis Grade ferrum est P11, P22, p9, P5, P91.
ASTM A335 P9 isaequalis to GB9948 or GB 6479 1Cr9Mo
ASTM A335 P22 isaequalis ad GB5310 12Cr2MoG
ASTM A335 P11 isaequalis ad GB5310 14Cr1MoG
ASTM A335 P5 isaequalis ad GB5310 1Cr5MoG
ASTM A335 P91 isaequalis ad GB5310 10Cr9Mo1VNbN
Differentia GB9948 et GB6479 in Application:
GB9948 est Seamless Ferro Tubuli pro PETROLEUM Cracking
GB6479 Seamless chalybe tubes for high-press Pro chemicis stercorat apparatibus
Sequentia No. | Test items ut | Test modus | Quantitas ad sampling | Standard |
1 | Chemical compositione | GB/T222 GB/T223 GB/4336 | Unum specimen pro se fornacem | GB6479/GB9948 |
2 | Test distrahentes | GB/T 228 | Unum specimen respectively ex duo fistulae cuiusque batch | GB6479/GB9948 |
3 | Test impulsum | GB/T 229 | Tria exempla respectively capta ex duobus tubulis cuiusque massam | GB6479/GB9948 |
4 | HYDRAULICUS test | GB/T 241 | Pars a piece | GB6479/GB9948 |
5 | Torcular-plana test | GB/T 246 | Unum specimen respectively ex duo fistulae cuiusque batch | GB6479/GB9948 |
6 | Opening expansion test | GB/T 242 | GB6479/GB9948 | |
7 | Humilis-complicare test | GB/T 226 GB/T 1979 | GB6479/GB9948 | |
8 | Non metallum inclusio | GB/T 10561 | GB6479/GB9948 | |
9 | Ultrasonic probatio | GB/T 5777 | Pars a piece | GB6479/GB9948 |
10 | Eddy probatio | GB/T 7735 | GB6479/GB9948 | |
11 | magnetica stillante probatio | GB/T 12606 | GB6479/GB9948 | |
12 | duritia Test | GB/T231.1 | Unum specimen respectively ex duo fistulae cuiusque batch | GB9949 |
Chemical Component
GB6479 | C | Si | Mn | Cr | Mo | V | Ti | NB | Ni | Cu | P | S |
1Cr5Mo | ≤0.15 | ≤0.5 | ≤0.6 | 4-6 | 0.45-0.6 | / | / | / | ≤0.6 | ≤0.2 | ≤0.03 | ≤0.03 |
GB9948 | C | Si | Mn | Cr | Mo | V | Ti | NB | Ni | Cu | P | S |
1Cr5Mo | ≤0.15 | ≤0.5 | ≤0.6 | 4-6 | 0.45-0.6 | / | / | / | ≤0.6 | ≤0.2 | ≤0.03 | ≤0.02 |
Chemical Component
Gradus | UN | C≤ | Mn | P≤ | S≤ | Si≤ | Cr | Mo |
Sequiv. | ||||||||
P1 | K11522 | 0.10~0.20 | 0.30~0.80 | 0.025 | 0.025 | 0.10~0.50 | - | 0.44~0.65 |
P2 | K11547 | 0.10~0.20 | 0.30~0.61 | 0.025 | 0.025 | 0.10~0.30 | 0.50~0.81 | 0.44~0.65 |
P5 | K41545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P5b | K51545 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.00~2.00 | 4.00~6.00 | 0.44~0.65 |
P5c | K41245 | 0.12 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 4.00~6.00 | 0.44~0.65 |
P9 | S50400 | 0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.50~1.00 | 8.00~10.00 | 0.44~0.65 |
P11 | K11597 | 0.05~0.15 | 0.30~0.61 | 0.025 | 0.025 | 0.50~1.00 | 1.00~1.50 | 0.44~0.65 |
P12 | K11562 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 0.80~1.25 | 0.44~0.65 |
P15 | K11578 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 1.15~1.65 | - | 0.44~0.65 |
P21 | K31545 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 2.65~3.35 | 0.80~1.60 |
P22 | K21590 | 0.05~0.15 | 0.30~0.60 | 0.025 | 0.025 | 0.5 | 1.90~2.60 | 0.87~1.13 |
P91 | K91560 | 0.08~0.12 | 0.30~0.60 | 0.02 | 0.01 | 0.20~0.50 | 8.00~9.50 | 0.85~1.05 |
P92 | K92460 | 0.07~0.13 | 0.30~0.60 | 0.02 | 0.01 | 0.5 | 8.50~9.50 | 0.30~0.60 |
Nova designatio ad normam E 527 et SAE J 1086, Usu ad Metalla Numerandi et Alloys (UNS). B Gradus P 5c contentum contentum carbo non minus quam 4 vicibus habeat nec plus quam 0,70%; vel columbium contentum 8 ad 10 tempora carbonis contentum.
Mechanica Property
Mechanica proprietatibus | P1,P2 | P12 | P23 | P91 | P92,P11 | P122 |
distrahentes vires | 380 | 415 | 510 | 585 | 620 | 620 |
cede vires | 205 | 220 | 400 | 415 | 440 | 400 |
Calor Curatio
Gradus | Caloris Curatio Type | Temperature Range F [C] | Subcritical Annealing vel Tempering |
P5, P9, P11 et P22 . | Temperature Range F [C] | ||
A335 P5 (b, c). | Plena vel Isothermal Anneal | ||
Normalize et ingenium | ***** | 1250 [675] | |
Subcritical Anneal (P5c only) | ***** | 1325-1375 [715 - 745]. | |
A335 P9 | Plena vel Isothermal Anneal | ||
Normalize et ingenium | ***** | 1250 [675] | |
A335 P11 | Plena vel Isothermal Anneal | ||
Normalize et ingenium | ***** | 1200 [650] | |
A335 P22 | Plena vel Isothermal Anneal | ||
Normalize et ingenium | ***** | 1250 [675] | |
A335 P91 | Normalize et ingenium | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
Exstingue et tempera | 1900-1975 [1040 - 1080] | 1350-1470 [730 - 800] |
Test opus est
Praeter compositionem chemicam et proprietates mechanicas praestandi, experimenta hydrostatica singillatim peraguntur, Examen non destruens , Product Analysis , Structura metallica et Testimenta Etching , Test adulatione etc.
Facultates copia
Facultates copia: MM Tons Per mense Per Grade ASTM A335 Admisce Ferro Pipe
Packaging
In manipulis et in ligneis Box
Delivery
7-14 dies, si in stirpe, 30-45 dies ad producendum
Payment
30% depsoit, 70% L/C vel B/L exemplum vel 100% L/C ad aspectum